耐老化性
TPE在很多不同条件下,如在水雾、臭氧、室外大气老化等条件下,化学稳定性优良。象大多数弹性体一样,在紫外光作用下会发生降解,对于室外应用或制品受阳光照射的条件,配方中应添加紫外光防护助剂,其中包括炭黑和各种颜料或其它屏蔽材料;TPE还具有不同程度的水解性。
荷兰DSM TPE Arnitel同系列型号介绍
Arnitel CM551 Heat Resistant Copolyester
Arnitel CM600-V 60 Shore D, Extrusion, Flame Retardant
Arnitel E2-UV Black color only, TPC based, UV masterbatch
Arnitel EL550 53 Shore D, Injection Molding
Arnitel EM550 53 Shore D, Extrusion Grade
Arnitel EM400 34 Shore D, Injection Molding or Extrusion Grade
Arnitel EM460 46 Shore D, Injection Molding or Extrusion Grade
Arnitel EL740 72 Shore D, Injection Molding
Arnitel PL380 33 Shore D, Injection Molding
Arnitel PL381 33 Shore D, Injection Molding
Arnitel PL461 46 Shore D, Injection Molding
Arnitel UM551-V 55 Shore D, Flame Retardant
Arnitel PM581 55 Shore D, Extrusion Grade
Arnitel PL460-S 46 Shore D, Injection Molding, Flame Retardant