Minlon 73GM40 NC010
PA6-(MD+GF)40
40%矿物/玻纤增强,热稳定,尼龙6
Minlon 73M30 NC010
PA6- MD30
30%矿物增强,热稳定,尼龙6
Minlon 73M40 NC010
PA6- MD40
40%矿物增强,热稳定,尼龙6
Zytel 7301 NC010
PA6
未增强尼龙6
Zytel 7304 NC010
PA6
未增强尼龙6
Zytel 7331J NC010
PA6
未增强尼龙6,
Zytel 7335F NC010
PA6
未增强尼龙6
Zytel 73G15HSL BK363
PA6-GF15
15%玻纤增强,热稳定,尼龙6
Zytel 73G15L NC010
PA6-GF15
15%玻纤增强尼龙6
Zytel 73G30HSL BK261
PA6-GF30
30%玻纤增强,热稳定,尼龙6
Zytel 73G30HSL BK416
PA6-GF30.
30%玻纤增强,热稳定,尼龙6
Zytel 73G30HSL NC010
PA6-GF30
30%玻纤增强,热稳定,尼龙6
Zytel 73G30L NC010
PA6-GF30
30%玻纤增强尼龙6
Zytel 73G30T BK261
PA6-I-GF30
30%玻纤增强,增韧,尼龙6
Zytel 73G30T NC010
PA6-I-GF30
30%玻纤增强,增韧,尼龙6
Zytel 73G30TGI BK267
PA6-I-GF30
30%玻纤增强,增韧,尼龙6
Zytel 73G35HSL BK262
PA6-GF35
35%玻纤增强,热稳定,尼龙6
Zytel 73G40T BK416
PA6-I-GF40
40%玻纤增强,增韧,尼龙6
Zytel 73G45 BK263
PA6-GF45
45%玻纤增强尼龙6
Zytel 73G45L NC010
PA6-GF45
45%玻纤增强尼龙6
Zytel 73G50HSLA BK416
PA6-GF50.
50%玻纤增强,热稳定,尼龙6
Zytel 74G33J NC010
(PA66+ PA6)-GF33
33%玻纤增强尼龙66+尼龙6
Zytel 74G33W BK196
(PA66+ PA6)-GF33
33%玻纤增强,耐UV,尼龙66+尼龙6
Zytel 74G33W NC010
(PA66+ PA6)-GF33
33%玻纤增强,耐UV,尼龙66+尼龙6
Zytel 84G33 BKB031
(PA66+ PA6)-I-GF3333% 玻纤增强,增韧,尼龙66+尼龙6
注意事项
1、PA6容易受潮,含水量对其力学性能有较大的影响。在熔融状态下,水分的存在,会引起其水解而导致分子量
下降,使制品机械性能下降,还会在成型中使制品表面出现气泡、银丝和斑纹等缺陷。成型前必须充分干
燥。
2、PA6熔体粘度低、流动性大,喷嘴会产生“流延”现象。浪费原料,污染喷嘴。如果用螺杆式注射机成型,
注射时,熔体会在螺杆和料筒壁之间出现逆流,使注料不准,PA6在螺杆式注射机成型时,在螺杆端部必
须安装止逆环。
3、PA6是结晶性高聚物。熔点明显,较高,尼龙6需要在较高温度下成型,熔融状态的尼龙6热稳定
性较差,易分解。必须严格控制工艺条件。
4、PA6的成型收缩率大,对于制造高精密度的制品,模具设计应在试验的基础上确定其尺寸,成型工艺应严格
控制。